HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 80281Generated: October 29, 2026
Sulfur Dioxide → HCID 131731886, compound
https://huagongshe.com/reaction/80281
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Sulfur Dioxide | HCID 1119 | — |
| Reactant | Azobisisobutyronitrile | HCID 6547 | — |
| Reactant | HCID 131731887 | HCID 131731887 | — |
| Solvent | Methanol | HCID 887 | — |
| Product | HCID 131731886 | HCID 131731886 | — |
Reaction Steps
Into a 300 ml-four-necked flask equipped with a stirrer, a thermometer, and a reflux condenser, a 1 mol/L diallyldimethylamine hydrochloride/diemthylsulfoxide (100 ml) and a 1 mol/L sulfur dioxide/diemthylsulfoxide solution (100 ml) were added and mixed, and azobis-isobutylonitrile (0.82 g) was added as a polymerization initiator to the mixture, followed by polymerizing at 40° C. for 24 hours. The reaction solution was added dropwise to methanol to precipitate the copolymer, filtered through a glass filter, followed by drying under reduced pressure, thereby obtaining 18 g of a copolymerized polymer (Production Example A-4). A weight average molecular weight of the copolymer determined by GPC (Gel Permeation Chromatography) (polyethylene glycol used as a standard) was about 3,000. The repeating unit of this polymer gas the following formula.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08845800B2 |
|---|
| Source dataset | uspto-grants-2014_09 |
|---|
| ORD ID | ord-eeee6c751c7840569337c559a09db0a4 |
|---|
| Source note | uspto-grants-2014_09 |
|---|