HRID83947

反应详情

EQUATION

反应方程式

HRID 83947 的结构方程式

PROCEDURE

实验过程

Similar to Example 51, with the following exception: 3.390 g (3.46×10−2 mol) α-methylene-γ-butyrolactone and 1.075 g (8.39×10−3 mol) n-butyl acrylate were used in the monomer mixture, yielding a polymer with a glass transition temperature of 145° C. Comparison to the Fox equation suggests the statistical copolymer contains approximately 11% n-butyl acrylate repeat units.

WORKUP

后处理

  1. customyielding a polymer with a glass transition temperature of 145° C