関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Terephthalic Acid | HCID 7489 | — |
| 溶媒 | Ethylene Glycol | HCID 174 | — |
| 生成物 | Bis(2-hydroxyethyl) terephthalate | HCID 13739 | — |
反応手順
Terephthalic acid was reacted with ethylene glycol to form bis-(2-hydroxyethyl) terephthalate and low oligomers thereof, in a standard direct esterification reaction. At the end of the direct esterification reaction 400 ppm of phosphoric acid stabiliser was added, followed by 500 ppm of antimony trioxide polycondensation catalyst and 500 ppm of "Irganox 1010" antioxidant. 0.3% of silica of particle size 4 μm, and 0.3% of titanium dioxide of particle size 0.2 μm were also added at this stage. A standard batch polycondensation reaction was performed until the intrinsic viscosity of the resultant polyethylene terephthalate was approximately 0.52. The polyethylene terephthalate was further polymerised by means of a batch solid phase polymerisation process, until the intrinsic viscosity (IV) of the polyethylene terephthalate was approximately 0.7 to 0.75. The solid phase polymerisation process utilised a fluidised bed, fluidised with nitrogen.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US05562984 |
|---|
| 出典データセット | uspto-grants-1996_10 |
|---|
| ORD ID | ord-a2f9a7b3f9b94e5eb5167e5bd5f93d65 |
|---|
| 出典メモ | uspto-grants-1996_10 |
|---|