HuagongsheHuagongshe Chemistry Print Report · For research reference only
Isobutylene → N-methylmaleimide isobutene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Isobutylene | HCID 8255 | — |
| Reactant | N-Methylmaleimide | HCID 70261 | — |
| Reactant | Neodecanoate | HCID 21225528 | — |
| Solvent | Toluene | HCID 1140 | — |
| Product | N-methylmaleimide isobutene | HCID 66864019 | — |
Reaction Steps
In a one-liter autoclave were charged 400 ml of toluene as a polymerization solvent, 0.001 moles of perbutyl neodecanoate as a polymerization initiator, 0.42 moles of N-methylmaleimide, and 4.05 moles of isobutene, and the mixture was subjected to polymerization reaction under a polymerization condition at a polymerization temperature of 60° C. for a polymerization time of 5 hours, to obtain N-methylmaleimide-isobutene alternating copolymer. The thus obtained N-methylmaleimide-isobutene alternating copolymer had a weight average molecular weight (Mw) (as reduced into standard polystyrene) of 165,000 and an Mw/Mn of 2.6.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US07001967B2 |
| Source dataset | uspto-grants-2006_02 |
| ORD ID | ord-aecbe2064ad24c798523ce957c5cb948 |
| Source note | uspto-grants-2006_02 |