HRID892712
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
PROCEDURE
实验过程
The polymerization of Example 10 was repeated except that in place of the organoaluminum oxy-compound, there were used 1 mmole of triisobutylaluminum and 1.4×10-3 mg atom in terms of titanium atom of the solid catalyst component [I], whereby 46.6 g of an ethylene/4-methyl-1-pentene copolymer having MFR of 0.01 g/10 min, a density of 0.912 g/cm3, an amount of decane-soluble portion of 0.10% by weight and Mw/Mn of 13.6 was obtained.
WORKUP
后处理
- customThe polymerization of Example 10
- customMFR of 0.01 g/10 min