HuagongsheHuagongshe Chemistry Print Report · For research reference only
Stearic Acid → Oleic Acid
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Stearic Acid | HCID 5281 | — |
| Reactant | Potassium Carbonate | HCID 11430 | — |
| Solvent | Water | HCID 962 | — |
| Product | Oleic Acid | HCID 445639 | 1% |
Reaction Steps
A solution containing 67.8% water, 1.2% of potassium carbonate, 25% paraffin, 5% stearic acid and 1% oleic acid is formed by melting the stearic acid, oleic acid and paraffin at about 90° to 100° C. and adding an aqueous solution of the potassium carbonate at 90° to 100° C. The resultant solution is stirred for more than 10 minutes at the temperature of 90° to 100° C. in a mixer at 1500 to 3600 r.p.m. until the apparent volume swells to about twice the original volume. This well stirred solution is cooled to 25° C. under stirring.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04230694 |
| Source dataset | uspto-grants-1980_10 |
| ORD ID | ord-2ffaea0679474c7eb8139a20cc22fdde |
| Source note | uspto-grants-1980_10 |