HuagongsheHuagongshe Chemistry Print Report · For research reference only
Water → Carbon Dioxide
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Water | HCID 962 | — |
| Reactant | Methyl morpholine oxide | HCID 82029 | — |
| Product | Carbon Dioxide | HCID 280 | — |
| Product | Formaldehyde | HCID 712 | — |
| Product | 4-Methylmorpholine | HCID 7972 | — |
| Product | Morpholine | HCID 8083 | — |
Reaction Steps
Additionally, amine-oxides, and particularly NMMO, have a limited thermal stability, which varies depending on their structure. The monohydrate of NMMO melts at temperatures of approximately 72° C., and the water-free compound melts at 172° C. When the monohydrate is heated, strong discolourings will occur from a temperature of 120°/130° C. on. Such temperatures however are common in processes for the production of cellulose moulded bodies. From 175° C. on, strong exothermal reactions will occur, which may lead to explosions. During this reaction, NMMO is thermally degraded, producing particularly N-methyl-morpholine, morpholine, formaldehyde and CO2.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05766530 |
| Source dataset | uspto-grants-1998_06 |
| ORD ID | ord-3a2afcb99b15455dad1cefcac609636d |
| Source note | uspto-grants-1998_06 |