Phosphoric Acid → Tricalcium Phosphate

https://huagongshe.com/reaction/973358

Reaction equation

Participants

RoleNameHCIDCharge
ReactantPhosphoric AcidHCID 1004—
ReactantCalcium CarbonateHCID 10112—
ProductTricalcium PhosphateHCID 24456—

Reaction Steps

Twenty kilograms of CaCO3 was mixed with 44 kg of H3PO4 (89%) and the resulting mixture was fired at 1,300° C. for 2 hours. The atomic Ca/P ratio in the fired product was about 0.5. The fired product was ground into a powder so that the particles of 5 μm or greater in size would be 40% on trommel. The powder was put into a 1% aqueous solution of methyl cellulose and stirred to form a calcium phosphate slurry. The previously prepared base material was immersed in the slurry and thereafter dried and fired in air atmosphere at 700° C. to have the surface of the base material covered with the first layer of calcium phosphate.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05062798
Source datasetuspto-grants-1991_11
ORD IDord-e428113040bb49908ebc2bcd6a91e710
Source noteuspto-grants-1991_11