化工社化工社 化学情報印刷レポート · 研究参考用
Acrylamide → Isooctyl Acrylate Acrylamide Vinyl Acetate
関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|---|---|---|
| 反応物 | Acrylamide | HCID 6579 | — |
| 反応物 | Vinyl Acetate | HCID 7904 | — |
| 反応物 | 2,2'-Azobis(2,4-dimethylvaleronitrile) | HCID 91537 | — |
| 反応物 | Isooctyl acrylate | HCID 165746 | — |
| 溶媒 | Methanol | HCID 887 | — |
| 溶媒 | Ethyl Acetate | HCID 8857 | — |
| 溶媒 | Ethylacetate methanol | HCID 21584119 | — |
| 生成物 | Isooctyl Acrylate Acrylamide Vinyl Acetate | HCID 86608178 | — |
反応手順
A master batch was prepared by combining isooctyl acrylate (621.0 g), acrylamide (41.4 g), vinyl acetate (165.6 g), 2,2'azobis(2,4-dimethylpentanenitrile) (1.656 g, VAZO™ 52, DuPont), ethyl acetate (884.5 g) and methanol (87.48 g). A portion (400 g) of the resulting solution was placed in a one quart (0.95 L) amber glass bottle. The bottle was purged for 2 minutes with nitrogen at a flow rate of 1 L/min. The bottle was sealed and placed in a rotary water bath at 45° C. for 24 hours to effect essentially complete polymerization. The copolymer was diluted with ethyl acetate: methanol (90:10 v/v) to 26.05% solids and had an inherent viscosity of 1.27 deciliter/gram in ethyl acetate at 0.15 g/deciliter.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 特許番号 | US05614210 |
| 出典データセット | uspto-grants-1997_03 |
| ORD ID | ord-f7a89e0d666f4ea1b31e9d1dd69fc52f |
| 出典メモ | uspto-grants-1997_03 |