Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 981793Generated: October 31, 2026

1-Octene → Silane, decylmethyldioctyl-

https://huagongshe.com/reaction/981793

Reaction equation

Participants

RoleNameHCIDCharge
Reactant1-OcteneHCID 8125—
ReactantHCID 123920282HCID 123920282—
CatalystRhodiumHCID 23948—
ProductSilane, decylmethyldioctyl-HCID 158304—

Reaction Steps

There was added 40 grams of methyldecylsilane for a period of 25 minutes to a mixture of 95.5 parts of 1-octene and 8 parts per million of rhodium catalyst as prepared in Example 2. A slow stream of air bubbled into the solution prior to the addition of the methyldecylsilane. The octene solution containing the rhodium catalyst was also preheated to a temperature of 80° C. After an additional 30 minutes of heating, an additional amount of rhodium catalyst was added to the mixture for a final total of 17 parts per million. After 1/2 hour, a quantitative yield of methyldecyldioctylsilane was obtained.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04992573
Source datasetuspto-grants-1991_02
ORD IDord-74f2bd62cf38499ca1e3589c50f9cb41
Source noteuspto-grants-1991_02