To a 50 mL beaker was added 16 g of urea-phosphate produce as above and 22 g Milli-Q™ water. The solids were stirred with a magnetic stirrer until dissolved. This solution was subsequently added dropwise to the Colloid BP slurry at a mixing speed of 800 rpm. The dispersion quickly increased in viscosity following the addition of the urea-phosphate solution. After 10 minutes of mixing the shear thinning product was prepared.
WORKUP
后处理
- dissolutionuntil dissolved
- additionThis solution was subsequently added dropwise to the Colloid BP slurry at a mixing speed of 800 rpm
- temperatureThe dispersion quickly increased in viscosity
- additionAfter 10 minutes of mixing the shear thinning product