Etidronic Acid → ZINC etidronate

HRID 1089373

Reaktionsgleichung

Reaktionsgleichung von HRID 1089373
[CH3:1][C:2]([P:8]([OH:11])([OH:10])=[O:9])([P:4]([OH:7])([OH:6])=[O:5])[OH:3].[O-2].[Zn+2:13]>>[Zn:13].[CH3:1][C:2]([P:8]([OH:11])([OH:10])=[O:9])([P:4]([OH:7])([OH:6])=[O:5])[OH:3]

Komponenten

3

Versuchsvorschrift

First, 790 g of a solution of etidronic acid (158 g as etidronic acid) was heated to 70° C. and 461 g of a zinc oxide slurry (92.2 g as zinc oxide) held at 70° C. was added dropwise over about 30 minutes with constant stirring. The mol ratio of zinc oxide to etidronic acid was 1.5/1. This slurry was stirred at 60° to 70° C. for 4 hours, after which it was cooled to room temperature. The slurry was then filtered and the dehydrated cake was washed with distilled water 3 to 5 times. It was then filtered, dried and pulverized to give zinc etidronate.

Aufarbeitung

  1. customheld at 70° C.
  2. additionwas added dropwise over about 30 minutes with constant stirring
  3. filtrationThe slurry was then filtered
  4. washthe dehydrated cake was washed with distilled water 3 to 5 times
  5. filtrationIt was then filtered
  6. customdried

Quellen und Nachweise

ORD-Eintrag
ord-693616ad3a774054a7b8c320fe4be31f
Quelldatensatz
uspto-grants-1990_10
Patentnummer
US04966630

Verknüpfte Notizen

Wird geladen…