Reaktionsgleichung
[CH2:1]=[C:2]=[CH2:3].[C:4]1([C:10]#[CH:11])[CH:9]=[CH:8][CH:7]=[CH:6][CH:5]=1.C=C=C.C#CC>CO>[CH2:1]=[C:2]=[CH2:3].[C:4]1([C:10]#[CH:11])[CH:9]=[CH:8][CH:7]=[CH:6][CH:5]=1Komponenten
5
Edukt 3
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 1
Reaktionsbedingungen
- Temperatur
- 60 °C
Versuchsvorschrift
In this example the starting monomers allene and phenylacetylene (HC≡C--O) are introduced into the catalyst mixture of Example 1 in a feed ratio of 62 to 38 (mole ratio). The polymerization conditions and catalyst are the same as in Example 1. After stirring at 60° C. for ten hours, a copolymer with a molecular weight of about 25,000 daltons (measured by GPC) is produced and can be isolated by precipitation to methanol. Given a starting amount of 0.5 g allene and 1.18 g phenylacetylene, the yield of copolymer will be 1.5 g, and have the formula: ##STR13##
Aufarbeitung
- customThe polymerization conditions and catalyst
- customa copolymer with a molecular weight of about 25,000 daltons (measured by GPC) is produced
Quellen und Nachweise
- ORD-Eintrag
- ord-6c267fdb1d9f4bf690b4a64c6c6aacaf
- Quelldatensatz
- uspto-grants-1998_05
- Patentnummer
- US05747618
Verknüpfte Notizen
Wird geladen…