[CH3:1][N:2]([CH3:6])[CH2:3][CH2:4][OH:5].C([CH:19]1[CH2:24][C:23](=[O:25])[O:22][C:20]1=[O:21])CCCCCCCCCCC>O=C1CC(C)(C)CC(C)=C1>[CH3:1][N:2]([CH3:6])[CH2:3][CH2:4][OH:5].[C:20]1(=[O:21])[O:22][C:23](=[O:25])[CH:24]=[CH:19]1Komponenten
5
Edukt 2
Produkt 2
Reagenzien, Katalysatoren, Lösungsmittel 1
Reaktionsbedingungen
- Temperatur
- 70 °C
Versuchsvorschrift
A reaction vessel containing 53.5 parts of Polyepoxide A (80 percent solids in isophorone) was heated to 70°C. There were added 3 parts of an amine produced by reacting dimethylethanolamine with dodecylsuccinic anhydride, and then there were added 6 parts of a second amine produced from dimethylethanolamine and maleic anhydride. During the second addition the temperature was raised to 95°C. and stirring was continued for 15 minutes at this temperature. The product when diluted with water and electrodeposited, as in the above examples, provided an adherent solvent-resistant coating.
Aufarbeitung
- customproduced
Quellen und Nachweise
- ORD-Eintrag
- ord-664b2dbd034848599956c811643f942d
- Quelldatensatz
- uspto-grants-1977_01
- Patentnummer
- US04001101
Verknüpfte Notizen