[Na+].[CH2:2]([C:14]1[CH:19]=[CH:18][CH:17]=[CH:16][C:15]=1S([O-])(=O)=O)[CH2:3][CH2:4]CCCCCCCCC.[C:24]([OH:28])(=[O:27])[CH:25]=[CH2:26]>O>[CH2:3]=[CH:2][C:14]1[CH:19]=[CH:18][CH:17]=[CH:16][CH:15]=1.[C:24]([O:28][CH2:14][CH2:2][CH2:3][CH3:4])(=[O:27])[CH:25]=[CH2:26]An aqueous solution was prepared that contained dodecylbenzenesulfonic acid sodium salt (“SDBS”) (6 g), Na2S2O7 (1.42 g, 0.0059 mol), HOTEMPO (1.85 g, 0.0107 mol), acrylic acid (9 ml) and de-ionized water (1.2 L). To this was added 300 mL of the pre-polymer (prepared according to Example 1) and stirred for about 5 minutes. The mixture was then piston homogenized for one pass at about 700 BAR. The mini-emulsion was transferred to the 2 L PARR reactor and then deoxygenated by 10 pressurization/depressurization cycles with argon. The mini-emulsion was then heated to 135° C. After 1 hour at temperature, 8 ml of ascorbic acid (0.189 g/ml) was continuously added at a rate of 0.033 ml per minute over a 4-hour period. After a total of 6 hours at temperature the reaction was cooled to yield a poly(styrene/butyl acrylate) latex of Mn=13,000, Tg of ˜50C with a PD of 1.46 and particle size of ˜190 nm.