Reaktionsgleichung
[NH2:1][C@H:2]([C:7]([O-:9])=[O:8])[CH2:3][C:4]([OH:6])=[O:5].[Na+:10].N[C@H:12]([C:17]([O-])=[O:18])[CH2:13][C:14](O)=[O:15].[NH4+:20]>>[NH2:1][C@H:2]([C:7]([O-:9])=[O:8])[CH2:3][C:4]([O-:6])=[O:5].[Na+:10].[Na+:10].[C:17]1(=[O:18])[NH:20][C:14](=[O:15])[CH2:13][CH2:12]1Komponenten
4
Versuchsvorschrift
Thermal Polymerization of the 1:1 Equivalent Comonomeric Composition Prepared from the Solution of Monosodium Aspartate and Monoammonium Aspartate to Produce a Copolymer of Sodium Aspartate and Succinimide by Thermal Treatment at 220° C.
Aufarbeitung
- customThermal Polymerization of the 1:1 Equivalent Comonomeric Composition