Reaktionsgleichung
[C:1]([O:5][CH2:6][CH:7](O)C)(=[O:4])[CH:2]=[CH2:3].CC1C(N=C=O)=CC([N:17]=C=O)=CC=1>>[C:1]([OH:5])(=[O:4])[CH:2]=[CH2:3].[NH2:17][C:1]([O:5][CH2:6][CH3:7])=[O:4]Komponenten
3
Reaktionsbedingungen
- Temperatur
- 70 °C
Versuchsvorschrift
In a flask equipped with a stirring blade, 260 parts (2 mol) of 2-hydroxypropyl acrylate(molecular weight of 130) was charged and 174 parts (1 mol) of TDI (2,4-tolylene diisocyanate) was added dropwise. After heating to 70° C. while paying attention to heat generation, the reaction was conducted at the same temperature for 7 hours. After confirming the disappearance of absorption of NCO by infrared absorption spectrum, the reaction product was taken out to obtain a urethane acrylate (H-1) as a radical polymerizable oligomer (A1).
Aufarbeitung
- additionwas charged
- temperatureto heat generation
- customthe disappearance of absorption of NCO by infrared absorption spectrum
Quellen und Nachweise
- ORD-Eintrag
- ord-562bc125bbe84b298e82cd9f09432128
- Quelldatensatz
- uspto-grants-2005_02
- Patentnummer
- US06850682B2
Verknüpfte Notizen
Wird geladen…