Reaktionsgleichung
[C:1](#[N:4])[CH:2]=[CH2:3].[C:5]([O:10]CCO)(=[O:9])[C:6]([CH3:8])=[CH2:7]>>[CH2:3]=[CH:2][CH:1]=[CH2:5].[C:1](#[N:4])[CH:2]=[CH2:3].[C:5]([OH:10])(=[O:9])[C:6]([CH3:8])=[CH2:7].[OH:9][CH:5]=[CH2:6]Komponenten
5
Versuchsvorschrift
A polymer of butadiene, acrylonitrile and hydroxyethylene methacrylate was prepared, by conventional emulsion polymerization techniques at a temperature of 13° C. The polymer contained about 34 weight percent of acrylonitrile and about 1 weight percent of hydroxyethyl methacrylate.