O1[CH:3]([CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH3:9])[CH2:2]1.N(C(C)(C)C#N)=NC(C)(C)C#N>C=CCCCCCC.C=CC1C=CC=CC=1>[CH2:2]=[CH:3][C:4]1[CH:9]=[CH:8][CH:7]=[CH:6][CH:5]=1.[CH2:2]=[CH:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH3:9]The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer.