Reaktionsgleichung
[C:1]([O:6][CH2:7][CH2:8][CH2:9][Si:10]([O:15][CH3:16])([O:13][CH3:14])[O:11][CH3:12])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:17]([O:22][CH3:23])(=[O:21])[C:18]([CH3:20])=[CH2:19].N(C(C)(C)C#N)=NC(C)(C)C#N>C1(C)C(C)=CC=CC=1>[C:1]([O:6][CH2:7][CH2:8][CH2:9][Si:10]([O:15][CH3:16])([O:11][CH3:12])[O:13][CH3:14])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:17]([O:22][CH3:23])(=[O:21])[C:18]([CH3:20])=[CH2:19]Komponenten
5
Edukt 3
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 1
Reaktionsbedingungen
- Temperatur
- 100 °C
Versuchsvorschrift
An undercoating material was prepared as follows. A mixture of 20 parts gamma-methacryloxypropyltrimethoxysilane, 80 parts methyl methacrylate, 100 parts xylene, and 1.0 part azobisisobutyronitrile was mixed and then heated at 100° C. for 3 hours to give gamma-methacryloxypropyltrimethoxysilane-methyl methacrylate copolymer. Xylene was added to this copolymer to prepare an undercoating material having 40 percent solids and a viscosity of 150 cP.
Aufarbeitung
- customAn undercoating material was prepared
- additionwas mixed
Quellen und Nachweise
- ORD-Eintrag
- ord-dc9a556e96bc494d975002d8be24b594
- Quelldatensatz
- uspto-grants-1988_08
- Patentnummer
- US04761312