Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Water | HCID 962 | — |
| Edukt | Sulfuric Acid | HCID 1118 | — |
| Edukt | Triphenyl phosphite | HCID 7540 | — |
| Edukt | Propanoic acid, 3,3'-thiobis-, didodecyl ester | HCID 31250 | — |
| Edukt | o,p-Divinylphenol | HCID 18541843 | — |
| Produkt | Cumen hydroperoxide | HCID 53627471 | — |
Reaktionsschritte
Then, 58 g of styrenated phenol, 44 g of dilaurylthiodipropionate, and 58 g of triphenyl phosphite were added to the obtained polymer latex. The mixture was coagulated at 50° C. with an aqueous 0.25% sulfuric acid so that the latex/water ratio was 1/2, and the mixture was maintained at 85° C. for 5 minutes.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04604416 |
|---|
| Quelldatensatz | uspto-grants-1986_08 |
|---|
| ORD ID | ord-e1b29b3db5e546f98a7fb326188f4b59 |
|---|
| Quellennotiz | uspto-grants-1986_08 |
|---|