HRID364145
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
CONDITIONS
反应条件
- 温度
- 85 °C
PROCEDURE
实验过程
Then, 58 g of styrenated phenol, 44 g of dilaurylthiodipropionate, and 58 g of triphenyl phosphite were added to the obtained polymer latex. The mixture was coagulated at 50° C. with an aqueous 0.25% sulfuric acid so that the latex/water ratio was 1/2, and the mixture was maintained at 85° C. for 5 minutes.