Reaktionsgleichung
[O-2].[O-2].[O-2].[O-2].[O-2].[V+5:6].[V+5].[C:8]([OH:13])(=[O:12])[C:9]([OH:11])=[O:10]>O>[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[V+5:6].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[V+5:6]Komponenten
4
Edukt 2
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 1
Reaktionsbedingungen
- Temperatur
- 1300 °C
Versuchsvorschrift
Granulated alumina (8 - 16 mesh) is heated at 1300° C. for 4 hours. Ferric oxalate and vanadium pentoxide are suspended in 5 parts of water, heated to 80° C., and oxalic acid is added slowly to obtain a blue-colored vanadium oxalate solution. Sodium carbonate is added and the alumina is also placed in the solution. The mixture is dried over a water bath with agitation. While air is pumped in, it is indurated in a furnace at 400° C. for 16 hours to obtain the catalyst ready for use after cooling.
Aufarbeitung
- temperatureheated to 80° C.
Quellen und Nachweise
- ORD-Eintrag
- ord-6da2ccc1f8bf4eda96990b6fb29bf5ef
- Quelldatensatz
- uspto-grants-1977_12
- Patentnummer
- US04064072
Verknüpfte Notizen
Wird geladen…