Reaktionsgleichung
[C:1]([O-:14])(=[O:13])[CH2:2][CH2:3][CH2:4]CCCCCCCC.[C:15]([O-:28])(=[O:27])[CH2:16]CCCCCCCCCC.C([Sn+2]CCCC)CCC.C1C=CC(C(N=C=O)N=C=O)=CC=1.C1C(CC2C=CC(N=C=O)=CC=2)=CC=C(N=C=O)C=1.[O:70]1[CH2:74][CH2:73][CH2:72][CH2:71]1>>[CH2:4]([OH:27])[CH2:3][CH2:2][CH2:1][OH:14].[C:74]([OH:70])(=[O:13])[CH2:73][CH2:72][CH2:71][CH2:16][C:15]([OH:28])=[O:27]Komponenten
6
Reaktionsbedingungen
- Temperatur
- 60 °C
Versuchsvorschrift
0.5 g of dibutyltin dilaurate was added to a 60% strength by weight solution of 105 g of toluylene diisocyanate and 170.0 g of diphenylmethane 4,4'-diisocyanate in tetrahydrofuran, and the mixture was then heated to 60° C. At this temperature, a 60% strength by weight solution of 345 g of a polyesterol obtained from 1,4-butanediol and adipic acid and having a molecular weight of 1000, 1267.0 g of a polyesterol obtained from 1,6-hexanediol, adipic acid and terephthalic acid, 3.17 g of trimethylolpropane, 4.76 g of methyldiethanolamine, 72 g of diethoxylated bisphenol A and 25.1 g of 1,6-hexanediol in tetrahydrofuran was metered in over 2 hours.
Quellen und Nachweise
- ORD-Eintrag
- ord-0183b656b3e54e159225f2517def800d
- Quelldatensatz
- uspto-grants-1999_07
- Patentnummer
- US05922469
Verknüpfte Notizen