Acetate → Silver behenate

HRID 649491
Drucken

Reaktionsgleichung

Reaktionsgleichung von HRID 649491
C(Cl)Cl.[Ag:4].[C:5]1([CH3:11])[CH:10]=[CH:9][CH:8]=[CH:7][CH:6]=1.[CH2:12]([C:14]([CH3:16])=O)[CH3:13].[C:17]([O-:20])(=[O:19])[CH3:18]>C([O-])(=O)CCCCCCCCCCCCCCCCC.[Zn+2].C([O-])(=O)CCCCCCCCCCCCCCCCC>[C:17]([O-:20])(=[O:19])[CH2:18][CH2:13][CH2:12][CH2:14][CH2:16][CH2:13][CH2:12][CH2:14][CH2:16][CH2:7][CH2:6][CH2:5][CH2:10][CH2:9][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:5][CH3:11].[Ag+:4]
KomponentenVersuchsvorschriftAufarbeitungQuellen und NachweiseNotizen zur Reaktion

Komponenten

8

Edukt 6

HCID 175AcetateHCID 1140TolueneHCID 6344DichloromethaneHCID 6569Methyl Ethyl KetoneHCID 23954SilverHCID 178435161HCID 178435161, Verbindung

Produkt 1

HCID 164971
Silver behenate

Reagenzien, Katalysatoren, Lösungsmittel 1

HCID 11178Zinc StearateKatalysator

Versuchsvorschrift

A uniform dispersion was prepared by dispersing 3 g of zinc stearate, 15 g of triacetyl cellulose, and 500 ml of methylene chloride in a ball mill for 10 hours. One surface of a polyethylene terephthalate film was subjected to a corona discharging treatment, and the above-described dispersion was coated on the treated surface to form a backing layer of 0.5 μm in thickness. Then, on the opposite surface thereof was coated a coating liquid of 10 g of nitrocellulose dissolved in 300 ml of acetate and dried to form an interlayer of 0.3 μm in thickness. 3 g of silver benehate was added to 20 g of a mixture of toluene and methyl ethyl ketone (1/2 by volume ratio), and the mixture was dispersed for about 20 hours in a ball mill to provide a uniform silver behenate suspension. Then, a silver behenate emulsion was prepared by adding the following composition (I) to 1.5 g of the silver behenate suspension.

Aufarbeitung

  1. customA uniform dispersion was prepared
  2. customto form a backing layer of 0.5 μm in thickness
  3. customdried
  4. customto form an interlayer of 0.3 μm in thickness
  5. additionthe mixture was dispersed for about 20 hours in a ball mill

Quellen und Nachweise

ORD-Eintrag
ord-ecd9143188074d2db09a93301cdc5787
Quelldatensatz
uspto-grants-1988_04
DOI
10.6084/m9.figshare.5104873.v1
Patentnummer
US04740439

Notizen zur Reaktion