Water → alpha-Methylene-gamma-butyrolactone acrylonitrile p-styrene sulfonate

HRID 83953

Reaktionsgleichung

Reaktionsgleichung von HRID 83953
[C:1](#[N:4])[CH:2]=[CH2:3].[CH2:5]=[C:6]1[CH2:11][CH2:10][O:9][C:7]1=[O:8].[CH2:12]=[CH:13][C:14]1[CH:19]=[CH:18][C:17]([S:20]([O-:23])(=[O:22])=[O:21])=[CH:16][CH:15]=1.[Na+].O.C(OOC(C)(C)C)(C)(C)C>>[CH2:5]=[C:6]1[CH2:11][CH2:10][O:9][C:7]1=[O:8].[C:1](#[N:4])[CH:2]=[CH2:3].[CH2:12]=[CH:13][C:14]1[CH:15]=[CH:16][C:17]([S:20]([O-:23])(=[O:22])=[O:21])=[CH:18][CH:19]=1

Komponenten

6

Reaktionsbedingungen

Temperatur
160 °C

Versuchsvorschrift

To a high-pressure stainless steel reactor with overhead stirring is added 7.82 g (0.147 mol) of acrylonitrile, 7.82 g (7.97×10−2 mol) of α-methylene-γ-butyrolactone, 0.50 g (2.42×10−3 mol) of sodium p-styrene sulfonate and 36.88 g (2.05 mol) of water. The reactor is purged with nitrogen and 0.78 g (5.33×10−3 mol) di-tert-butyl peroxide is added to the reaction mixture before the reactor is tightly closed and heated to 160° C. After 10 minutes at 160° C., the polymerization is allowed to cool to room temperature before drying the polymer under vacuum at elevated temperature for isolation.

Aufarbeitung

  1. additionis added to the reaction mixture before the reactor
  2. customis tightly closed
  3. temperatureto cool to room temperature
  4. custombefore drying the polymer under vacuum at elevated temperature for isolation

Quellen und Nachweise

ORD-Eintrag
ord-3ce3c6904c8c4ded9cf8fea90d96f1ec
Quelldatensatz
uspto-grants-2014_09
Patentnummer
US08846817B2

Verknüpfte Notizen

Wird geladen…