Reaktionsgleichung
C(O)C.[OH-].[Na+].[CH:6]([N:8]1[CH2:12][CH2:11][CH2:10][C:9]1=[O:13])=[CH2:7].[C:14]([O:17][CH:18]=[CH2:19])(=[O:16])[CH3:15]>C(OCC)C>[CH:6]([N:8]1[CH2:12][CH2:11][CH2:10][C:9]1=[O:13])=[CH2:7].[C:14]([O:17][CH:18]=[CH2:19])(=[O:16])[CH3:15]Komponenten
6
Edukt 4
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 1
Reaktionsbedingungen
- Temperatur
- 30 °C
Versuchsvorschrift
Into a 2 liter round bottom flask 800 ml of ethanol, 12.8 g of sodium hydroxide pellets and 80 g of a copolymer composed of 70% N-vinylpyrrolidone and 30% vinyl acetate are introduced. The resulting reaction mixture is maintained with stirring at 30° C. for 2 hours and is then poured into 8 liters of diethyl ether to precipitate the desired polymer. After filtration the polymer is dried under reduced pressure. Yield: 95%.
Aufarbeitung
- additionare introduced
- customThe resulting reaction mixture
- temperatureis maintained
- customto precipitate the desired polymer
- filtrationAfter filtration the polymer
- customis dried under reduced pressure
Quellen und Nachweise
- ORD-Eintrag
- ord-89a3e98d71a44dd59f10265f058e1e6b
- Quelldatensatz
- uspto-grants-1981_08
- Patentnummer
- US04283384
Verknüpfte Notizen
Wird geladen…