[C:1]([C:5]1[CH:12]=[CH:11][C:8](C=C)=[CH:7][CH:6]=1)([CH3:4])([CH3:3])[CH3:2]>O>[C:1]([CH:5]1[CH2:12][CH2:11][CH2:8][CH2:7][CH2:6]1)([CH3:4])([CH3:3])[CH3:2]By using the same autoclave as used in Preparation Example 1, 300 g of p-tert-butylstyrene polymer (Mw=20.4×104, Mn=11.2×104, Mw/Mn=1.82) prepared by suspension polymerization in water, was charged instead of 300 g of polystyrene in Preparation Example 1. The hydrogenation reaction and post-treatment were conducted in the same manner as in Preparation Example 1 except that the hydrogenation conditions were changed as identified in Table 1, whereby polyvinyl p-tert-butylcyclohexane was obtained.