Reaction equation
[C:1]([NH2:5])(=[O:4])[CH:2]=[CH2:3].[C:6]([O:11][CH2:12][CH2:13][N:14]([CH2:17][CH3:18])[CH2:15][CH3:16])(=[O:10])[C:7]([CH3:9])=[CH2:8].Cl>>[C:1]([NH2:5])(=[O:4])[CH:2]=[CH2:3].[C:6]([O:11][CH2:12][CH2:13][N:14]([CH2:17][CH3:18])[CH2:15][CH3:16])(=[O:10])[C:7]([CH3:9])=[CH2:8]Participants
4
Procedure
The procedure described in Reference Example 1 was repeated except that 49.7 g. of acrylamide, 55.8 g. of diethylaminoethyl methacrylate and 31.3 g. of 35 % hydrochloric acid wre employed to give an aqueous solution of acrylamide-diethylaminoethyl methacrylate copolymer having a concentration of 9.9 %, a pH value of 4.6 and a viscosity of 4,500 cP at 25°C.
Sources & evidence
- ORD record
- ord-906985a46f1d43c6926be07eb685e6cc
- Source dataset
- uspto-grants-1976_08
- Patent number
- US03976824
Linked notes