HRID 1611566 reaction equation
[Ni:1].[Zn:2].[O-:3][P:4]([O:7][P:8]([O-:11])([O-:10])=[O:9])(=[O:6])[O-:5].[Zn+2].[Zn+2].S([O-])([O-])(=O)=O.[Ni+2].[O-]P(OP([O-])([O-])=O)(=O)[O-].[K+].[K+].[K+].[K+]>[Zn].[Ni].[Cu]>[O-:5][P:4]([O:7][P:8]([O-:11])([O-:10])=[O:9])(=[O:3])[O-:6].[Ni:1].[Zn:2]
ParticipantsProcedureWorkupSources & evidenceReaction notes

Participants

10

Reactant 5

HCID 935Nickel3×HCID 23740Potassium pyrophosphate2×HCID 23994Zinc3×HCID 24586Nickel SulfateHCID 62641Zinc pyrophosphate

Product 3

HCID 935Nickel
HCID 23994
Zinc
HCID 644102Pyrophosphate

Reagents, catalysts & solvents 2

HCID 23978CopperCatalystHCID 14877100Nickel--zinc (1/1)Solvent2×

Procedure

However, the composition of nickel and zinc in the nickel-zinc alloy layer 5 was purposely deviated from the range according to the present invention in which the content of nickel is 70 to 88 wt % and the content of zinc is the balance. Thus, for this nickel-zinc alloy layer 5, a pyrophosphate based solution was prepared using zinc pyrophosphate (ZnP2O7·3H2O), nickel sulfate (NiSO4·7H2O) and potassium pyrophosphate (K2P4O7) so that the solution had a composition with 0.6 g/l of zinc, 10.0 g/l of nickel and 100 g/l of potassium pyrophosphate, and in the solution at a liquid temperature of 30° C., the copper foil itself was made to undergo cathode polaraization with the use of a stainless plate for the counter electrode under conditions of current density of 0.8 A/dm2 and electrolysis time of 6000 seconds, thereby providing an alloy composition with 7.74 g/m2 (90.0 wt %) of nickel and 0.86 g/cm2 (10.0 wt %) of zinc. The weight thickness of the nickel-zinc alloy layer 5 was 8.60 g/m2. In concurrence with this formation of the nickel-zinc alloy layer 5 on the nodular treatment side 4, 0.02 g/m2 of nickel-zinc layer was formed on the shiny side 6 of the untreated copper foil 2 as a corrosion prevention layer.

Workup

  1. customat a liquid temperature of 30° C.
  2. customelectrolysis time of 6000 seconds

Sources & evidence

ORD record
ord-cdafc828e71a4776b57ff4849f87120c
Source dataset
uspto-grants-2006_01
DOI
10.6084/m9.figshare.5104873.v1
Patent number
US06989199B2

Reaction notes

On this pageParticipantsProcedureWorkupSources & evidenceReaction notes