Reaction equation
[CH2:1]1[O:4][CH:2]1[CH3:3].[CH2:5]1[O:9][CH2:8][CH2:7][CH2:6]1>OCC(CO)O.[OH-].[K+]>[CH2:1]1[O:4][CH:2]1[CH3:3].[CH2:8]1[O:9][CH2:5][CH2:6][CH2:7]1Participants
5
Reactant 2
Product 1
Reagents, catalysts & solvents 2
Procedure
In a 10 l autoclave, 92 g of glycerol, 24 g of potassium hydroxide, 6,970 g of propylene oxide and 1,100 g of butylene oxide were fed and reacted together at 110° C. for 15 hours. After the reaction has been completed, the mixture was neutralized and desalted to obtain 8,100 g of a trifunctional propylene oxide-butylene oxide random copolymer. Its molecular weight was 8,145 (calculated from its hydroxyl number).
Workup
- customreacted together at 110° C. for 15 hours
Sources & evidence
- ORD record
- ord-29f229fa44be4342acb73cc3b1a74133
- Source dataset
- uspto-grants-1995_07
- Patent number
- US05436090