Reaction equation
[C:1]([O:6][CH2:7][CH:8]([CH2:13][CH3:14])[CH2:9][CH2:10][CH2:11][CH3:12])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:15]([OH:20])(=[O:19])[C:16]([CH3:18])=[CH2:17].N(C(C)(C)C#N)=NC(C)(C)C#N>>[C:1]([O:6][CH2:7][CH:8]([CH2:13][CH3:14])[CH2:9][CH2:10][CH2:11][CH3:12])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:15]([OH:20])(=[O:19])[C:16]([CH3:18])=[CH2:17]Participants
4
Conditions
- Temperature
- 85 °C
Procedure
To the above solvent, a mixture of 200 g of 2-ethylhexyl methacrylate, 5 g of methacrylic acid and 3 g of azobisisobutyronitrile was added dropwise at a constant speed over a period of 2 hours, followed by stirring at 85° C. for 2 hours to complete the polymerization reaction. Thus, 2-ethylhexyl methacrylate - methacrylic acid copolymer was obtained.
Workup
- additionwas added dropwise at a constant speed over a period of 2 hours
- customthe polymerization reaction
Sources & evidence
- ORD record
- ord-f1f1a742d3c2412dbe2fb044ae9a8b1f
- Source dataset
- uspto-grants-1994_07
- Patent number
- US05328794
Linked notes
Loading…