Reaction equation
[C:1]1(=[O:7])[NH:5][C:4](=[O:6])[CH:3]=[CH:2]1.[CH:8]([O:10][C:11](=[O:19])[CH:12]([CH2:17][CH3:18])[CH2:13][CH2:14][CH2:15][CH3:16])=[CH2:9]>>[C:4]1(=[O:6])[NH:5][C:1](=[O:7])[CH:2]=[CH:3]1.[CH:8]([O:10][C:11](=[O:19])[CH:12]([CH2:17][CH3:18])[CH2:13][CH2:14][CH2:15][CH3:16])=[CH2:9]Participants
3
Procedure
A polymer was prepared in the manner of Example 1, except the comonomer to maleimide was vinyl-2-ethylhexanoate (vinyl ester) and the reaction time was 25 hours. The polymer yield was 57%.
Sources & evidence
- ORD record
- ord-34783edf7d494a16be555079ed4c068c
- Source dataset
- uspto-grants-1988_01
- Patent number
- US04720445
Linked notes