Reaction equation
[C:1]([OH:5])(=O)[CH:2]=[CH2:3].[C:6]([OH:10])(=O)[CH:7]=[CH2:8].[C:11](O)(=[O:14])C=C.C(C(CO)(CO)CC)O.C(C1C=C(CC)C2SC3C(=CC=CC=3)C(=O)C=2C=1)C>[O-][Ti]([O-])=O.[Ba+2].C(O)C>[CH3:11][O:14][CH:7]([CH2:6][O:10][CH:2]([CH2:1][OH:5])[CH3:3])[CH3:8]Participants
5
Procedure
A slurry obtained by mixing 6.2 g of a borosilicate glass powder, 56.0 g of barium titanate, 6.2 g of an acrylic organic binder containing hydroxyl groups, 3.1 g of ethanol, 3.0 g of trimethylolpropane triacrylate, 1.2 g of 2-methyl-1-[4-(methylthio)phenyl]-2-morphorinopropane-1-on, 0.3 g of 2,4-diethylthioxanthone and 0.5 g of dipropyleneglycol monomethyl ether was formed into a sheet by the doctor blade method. The sheet was dried at 100° C. to obtain a photosensitive dielectric ceramic green sheet with a thickness of 30 μm.
Workup
- customA slurry obtained
Sources & evidence
- ORD record
- ord-cfa2b1b5def348e7bcd074b938d77348
- Source dataset
- uspto-grants-2001_02
- Patent number
- US06183669B2
Linked notes
Loading…