[CH2:1](S)[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH3:12].CCCC[CH2:18][C:19]([C:23]([O:25]OC(C)(C)C)=[O:24])([CH2:21]C)[CH3:20]>C1(C)C=CC=CC=1>[C:23]([O:25][CH2:1][CH3:2])(=[O:24])[CH:19]=[CH2:21].[C:23]([O:25][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH3:12])(=[O:24])[C:19]([CH3:20])=[CH2:18]Participants
5
Reactant 2
Product 2
Reagents, catalysts & solvents 1
Procedure
350 g of toluene, 135 g of ethyl acrylate, and 15 g of n-decyl methacrylate were polymerized with stirring in a reaction flask at 50°-60° C. under argon with 0.3 g of dodecyl mercaptan as a regulator and 2 g of t-butyl perneodecanoate as initiator. After about 30 minutes of reaction, the mixture was precipitated in methanol and the polymer was dried under vacuum.
Workup
- customAfter about 30 minutes of reaction
- customthe mixture was precipitated in methanol
- customthe polymer was dried under vacuum
Sources & evidence
- ORD record
- ord-c2b49c75adc9482d84cd3eef32fdd950
- Source dataset
- uspto-grants-1992_08
- Patent number
- US05141993
Linked notes
Loading…