反応式
[C:1]([O-:20])(=[O:19])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13]CCCCC.[Na+].[C:22]([O-])(=[O:40])[CH2:23]CCCCCCCCCCCCCCCC.[K+].C([O:45]CCOCCO)C>>[C:13]1(=[O:45])[O:40][CH2:22][CH2:23][O:20][C:1](=[O:19])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12]1参加物
4
実験手順
A mixed metal catalyst prepared similarly to that of Example X, except that sodium stearate was substituted for the potassium stearate and ethyl cellusolve replaced with diethylene glycol monoethyl ether, was employed for the continuous depolymerization of poly(ethylene brassylate) in accordance with the procedure and conditions of Example I. Ethylene brassylate was continuously produced and distilled from the reactor at a rapid rate and the overall yield was 73.2%. Comparable results are obtained with a catalyst comprised of sodium benzoate and aluminum tricellusolve (Al(OCH2CH2OC2H5)3).
後処理
- customA mixed metal catalyst prepared similarly to that of Example X
出典と根拠
- ORDレコード
- ord-4a23ea2bd1114aa0b97a9174535b9e69
- 出典データセット
- uspto-grants-1983_07
- 特許番号
- US04393223
関連ノート
読み込み中…