Ethylene → Ethylene styrene

HRID 1256870
印刷

反応式

HRID 1256870 の反応式
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH2:9]=[CH2:10].CO.Cl>>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH2:9]=[CH2:10]
参加物実験手順後処理出典と根拠反応ノート

参加物

4

反応物 3

HCID 6325EthyleneHCID 7501StyreneHCID 21893726Hydrochloride methanol

生成物 1

HCID 22558332Ethylene styrene

実験手順

340 mL of dehydrated toluene, 50 mL of styrene and TIBA (1.8 mmol) were placed in a 1 L autoclave, which had been dried by heating, at room temperature under a nitrogen atmosphere. After making the temperature thereof to 70° C. under stirring, mL of a toluene solution of (9-ethyl-1,2,3,4-tetrahydro-1-fluorenyl)-bis(N,N-dimethylaminobenzyl)scandium obtained in the item (E) of Example 1 (0.027 mmol) and triphenylcarbenium tetrakispentafluorophenylborate (0.027 mmol), which had been mixed in advance, was added thereto. The mixture was homopolymerized for styrene for 5 minutes, and then further polymerized for 5 minutes while maintaining the pressure to 0.1 MPa with ethylene. After completing the polymerization reaction, the reaction product was placed in a methanol-hydrochloric acid solution, and after stirring sufficiently, the polymer was filtered off, sufficiently rinsed with methanol, and dried to provide 43 g of a styrene-ethylene copolymer.

後処理

  1. additionhad been mixed in advance
  2. additionwas added
  3. customfurther polymerized for 5 minutes
  4. customthe polymerization reaction
  5. filtrationthe polymer was filtered off
  6. washsufficiently rinsed with methanol
  7. customdried