Hydroxylapatite (Ca5(OH)(PO4)3) → Hydroxylapatite (Ca5(OH)(PO4)3)

HRID 129358

反応式

HRID 129358 の反応式
[OH-].[O-:2][P:3]([O-:6])([O-:5])=[O:4].[O-:7][P:8]([O-:11])([O-:10])=[O:9].[O-:12][P:13]([O-:16])([O-:15])=[O:14].[Ca+2:17].[Ca+2].[Ca+2].[Ca+2].[Ca+2].[N+]([O-])([O-])=O.[Ag+:26].[N+]([O-])([O-])=O.[Zn+2:31].[N+]([O-])([O-])=O>O>[OH-:2].[O-:9][P:8]([O-:11])([O-:10])=[O:7].[O-:14][P:13]([O-:16])([O-:15])=[O:12].[O-:4][P:3]([O-:6])([O-:5])=[O:2].[Ca+2:17].[Ca+2:17].[Ca+2:17].[Ca+2:17].[Ca+2:17].[Ag:26].[Zn:31]

参加物

7

実験手順

Hydroxylapatite in an amount of 1.0 kg is added to 10 liters of water together with 32 g of silver nitrate and 69 g of zinc nitrate, and then the whole was stirred to make a reaction. The solids are separated off to form a cake, then the cake is rinsed thoroughly with distilled water and dried. The washed cake is heated or fired at 1200° C. and powdered to provide the antibacterial hydroxylapatite carrying about 2% by weight of silver in a metallic state and 1.5% by weight of zinc in a metallic state.

後処理

  1. customa reaction
  2. customThe solids are separated off
  3. customto form a cake
  4. washthe cake is rinsed thoroughly with distilled water
  5. customdried
  6. temperatureThe washed cake is heated
  7. customfired at 1200° C.

出典と根拠

ORDレコード
ord-161a16f4c90c49ac99a95de7817dfeb0
出典データセット
uspto-grants-1995_11
特許番号
US05468489