[CH:1]1[CH:6]=[CH:5][C:4](/[CH:7]=[CH:8]/[CH2:9][O:10][C@@H:11]2[O:16][C@H:15]([CH2:17][OH:18])[C@@H:14]([OH:19])[C@H:13]([OH:20])[C@H:12]2[OH:21])=[CH:3][CH:2]=1.[CH2:22]1[CH:26]2[CH:27]3[CH:31]=[CH:30][CH:29]([CH:25]2[CH:24]=[CH:23]1)[CH2:28]3>>[CH:1]1[CH:2]=[CH:3][C:4](/[CH:7]=[CH:8]/[CH2:9][O:10][C@@H:11]2[O:16][C@H:15]([CH2:17][OH:18])[C@@H:14]([OH:19])[C@H:13]([OH:20])[C@H:12]2[OH:21])=[CH:5][CH:6]=1.[CH2:22]1[CH:26]2[CH:27]3[CH:31]=[CH:30][CH:29]([CH:25]2[CH:24]=[CH:23]1)[CH2:28]3参加物
3
反応条件
- 温度
- 260 °C
実験手順
Proportions of phenolic-modified rosin (from Example 1) and dicyclopentadiene, as indicated in Table II, were charged into a one-liter autoclave reactor. The charged autoclave was purged with nitrogen and sealed. The reaction mixture was heated to 260° C. within 60 minutes and maintained at 260° C. for six hours. The reactor then was vented carefully, and the molten resin poured into an aluminum pan and allowed to cool.
後処理
- additionwere charged into a one-liter autoclave reactor
- customThe charged autoclave was purged with nitrogen
- customsealed
- temperaturemaintained at 260° C. for six hours
- additionthe molten resin poured into an aluminum pan
- temperatureto cool