反応式

HRID 1731568 の反応式
[C:1]([OH:5])(=[O:4])[CH:2]=[CH2:3].N.[C:7]([NH2:11])(=[O:10])[CH:8]=[CH2:9]>O>[C:1]([OH:5])(=[O:4])[CH:2]=[CH2:3].[C:7]([NH2:11])(=[O:10])[CH:8]=[CH2:9]
参加物実験手順後処理出典と根拠反応ノート

参加物

5

反応物 3

HCID 222AmmoniaHCID 6579AcrylamideHCID 6581Acrylic Acid2 回

生成物 1

HCID 62693Acrylamide-acrylic acid resin

試薬・触媒・溶媒 1

HCID 962Water溶媒

実験手順

To a stainless steel beaker was charged 214 g. of glacial acrylic acid (Rohm and Haas Production Grade). While stirring with a magnetic stirrer, 29% aqueous ammonia (technical) was added and the temperature was maintained at ≤35° C. until the pH became 7.5 (about 1.5 hours). Distilled water was added to bring the total weight of 428 g. The solution was transferred to a 1 liter glass beaker and while stirring 1.07 g. of methone was added (0.5% based on the acrylic acid). It dissolved in about 10 minutes. Then 23 g. of 50% acrylamide was added and the procedure of Examples 29-38 was followed to emulsion polymerize the monomers.

後処理

  1. temperaturethe temperature was maintained at ≤35° C. until the pH
  2. custom7.5 (about 1.5 hours)
  3. stirringwhile stirring 1.07 g
  4. additionof methone was added (0.5%
  5. dissolutionIt dissolved in about 10 minutes
  6. custompolymerize the monomers

出典と根拠

ORDレコード
ord-a792d4a3e1b64ecb85298b817c0a2d6f
出典データセット
uspto-grants-1986_11
DOI
10.6084/m9.figshare.5104873.v1
特許番号
US04622356

反応ノート