N,N-diethyl-m-toluamide → Urea Urethane
反応式
CC([NH:4]P([O:9][C:10]1[CH:15]=CC(Cl)=CC=1Cl)(OC)=S)C.CC([N:33]=[C:34]=[O:35])(C1C=CC=C(C([N:30]=[C:31]=[O:32])(C)C)C=1)C.[OH-].[Na+].CCN(C(C1C=CC=C(C)C=1)=O)CC>O.CC(=O)OCC>[NH2:30][C:31]([O:9][CH2:10][CH3:15])=[O:32].[NH2:4][C:34]([NH2:33])=[O:35]参加物
7
実験手順
143.1 g of Rucoflex XS-5570-55, 154.4 g of Rucoflex S-1011-55, 9.0 g of MPdiol and 6.7 g of DMPA are reacted with 73.2 g of TMXDI and 25.2 d of HDI at 80° C. for 3 hours to prepare a prepolymer. The prepolymer is then dispersed in a solution of 3.0 NaOH and 2.75 g of EA in 736 g of water. After 5 minutes, a solution of 2.7 g of EDA and 3.06 g of DETA in 50.0 g of water is added to form a aqueous poly(urethane/urea) dispersion. A finely divided dispersion having solids content of 35.2% and a pH of 7.85 is obtained.
後処理
- customto prepare a prepolymer
出典と根拠
- ORDレコード
- ord-278dd2f947f74721b09b9fbac89b2b03
- 出典データセット
- uspto-grants-1997_12
- 特許番号
- US05703158
反応ノート
読み込み中…