戻る
化工社化工社 化学情報印刷レポート · 研究参考用
HRID 2120034作成日:2026年10月27日

Acetic Acid → 2-ethyl-2-adamantyl Methacrylate p-hydroxystyrene

https://huagongshe.com/reaction/2120034

反応式

関与物質

役割名称HCID仕込み量
反応物Acetic AcidHCID 176—
反応物4-Ethenylphenyl acetateHCID 75821—
反応物2-Ethyl-2-methacryloyloxyadamantaneHCID 9813645—
触媒4-(Dimethylamino)pyridineHCID 14284—
溶媒MethanolHCID 887—
生成物2-ethyl-2-adamantyl Methacrylate p-hydroxystyreneHCID 22508392—

反応手順

Into a flask were charged 250 g of the copolymer of 2-ethyl-2-adamantyl methacrylate and p-acetoxystyrene (30:70) obtained in Reference Example 7, 10.8 g (0.088 mol) of 4-dimethylaminopyridine and 239 g of methanol and the mixture was aged for 20 hours under reflux. After cooling, the reaction solution was neutralized with 8.0 g (0.133 mol) of glacial acetic acid, and precipitated by pouring into a large amount of water. The precipitated polymer was dissolved in acetone, then, poured into a large amount of water to cause precipitation. This operation was repeated three times in total, to effect purification. The amount of the resulted copolymer of 2-ethyl-2-adamentyl methacrylate and p-hydroxystyrene was 102.8 g. The weight-average molecular weight was about 8200, the degree of dispersion was 1.68 (GPC method: reduced by polystyrene), and the copolymerization ratio was determined to be about 30:70 by a nuclear magnetic resonance (13C-NMR) spectrometer. This resin is called resin A6.

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US06689531B2
出典データセットuspto-grants-2004_02
ORD IDord-7b4ba0d1c5034139a1b4072b94c52353
出典メモuspto-grants-2004_02