反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
AUXILIARIES
试剂、催化剂与溶剂
PROCEDURE
实验过程
Into a flask were charged 250 g of the copolymer of 2-ethyl-2-adamantyl methacrylate and p-acetoxystyrene (30:70) obtained in Reference Example 7, 10.8 g (0.088 mol) of 4-dimethylaminopyridine and 239 g of methanol and the mixture was aged for 20 hours under reflux. After cooling, the reaction solution was neutralized with 8.0 g (0.133 mol) of glacial acetic acid, and precipitated by pouring into a large amount of water. The precipitated polymer was dissolved in acetone, then, poured into a large amount of water to cause precipitation. This operation was repeated three times in total, to effect purification. The amount of the resulted copolymer of 2-ethyl-2-adamentyl methacrylate and p-hydroxystyrene was 102.8 g. The weight-average molecular weight was about 8200, the degree of dispersion was 1.68 (GPC method: reduced by polystyrene), and the copolymerization ratio was determined to be about 30:70 by a nuclear magnetic resonance (13C-NMR) spectrometer. This resin is called resin A6.
WORKUP
后处理
- temperatureunder reflux
- temperatureAfter cooling
- customprecipitated
- additionby pouring into a large amount of water
- dissolutionThe precipitated polymer was dissolved in acetone
- additionpoured into a large amount of water
- customprecipitation
- custompurification