反応式
[N-:1]=[C:2]=[O:3].[N-]=C=O.C1(CC2C=CC=CC=2)C=CC=CC=1.[C:20]([O-])(=[O:32])[CH2:21]CCCCCCCCCC.C([O-])(=O)CCCCCCCCCCC.C([Sn+2]CCCC)CCC.[C:57]([O:62]CCO)(=[O:61])[C:58]([CH3:60])=[CH2:59]>>[C:57]([OH:62])(=[O:61])[C:58]([CH3:60])=[CH2:59].[C:57]([OH:62])(=[O:61])[C:58]([CH3:60])=[CH2:59].[NH2:1][C:2]([O:32][CH2:20][CH3:21])=[O:3]参加物
4
反応条件
- 温度
- 70 °C
実験手順
100 Parts of polyesterdiol which was formed from butanediol and adipic acid and had a molecular weight of about 1,000, 75 parts of diphenylmethane diisocyanate and 0.1 part of dibutyltin dilaurate were mixed, and the resultant mixture was allowed to react at 50° C. for 30 minutes and at 90° C. for 2 hours, and the reaction mixture was cooled to 70° C. Then, 26 parts of 2-hydroxyethyl methacrylate was added, and further, the resultant mixture was allowed to react for 3 hours to give urethane dimethacrylate.
後処理
- additionwere mixed
- customto react at 50° C. for 30 minutes and at 90° C. for 2 hours
- customto react for 3 hours
出典と根拠
- ORDレコード
- ord-76eb127d6b84468fbc3676b966fc5b4f
- 出典データセット
- uspto-grants-1994_11
- 特許番号
- US05362604