反応式
[CH:1]([S:9]([O-:12])(=[O:11])=[O:10])=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[Na+].[F:14][C:15]([F:37])=[C:16]([F:36])[C:17]([F:35])([F:34])[C:18]([F:33])([F:32])[C:19]([F:31])([F:30])[C:20]([F:29])([F:28])[C:21]([F:27])([F:26])[C:22]([F:25])([F:24])[F:23].N(C(C)(C)C#N)=NC(C)(C)C#N>CS(C)=O>[CH:1]([S:9]([O-:12])(=[O:10])=[O:11])=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[F:14][C:15]([F:37])=[C:16]([F:36])[C:17]([F:34])([F:35])[C:18]([F:32])([F:33])[C:19]([F:30])([F:31])[C:20]([F:29])([F:28])[C:21]([F:27])([F:26])[C:22]([F:25])([F:24])[F:23]参加物
5
実験手順
16 g of sodium styrenesulfonate (SSNa) (available from Sigma-Aldrich Corp.) and 4 g of perfluorooctene (1H,1H,2H-perfluoro-1-octene) are fully dissolved in 0.24 L of dimethylsulfoxide (DMSO) with heating. Then, 0.1 g of azobisisobutyronitrile (AIBN) is added dropwise to the DMSO solution. The monomers are polymerized for 24 hours or more. The polymerization is carried out varying the content of perfluorooctene (5, 10, and 20 wt %). The reaction product is allowed to sit at ambient temperature. Then, a precipitate is colleted from the reaction product and filtered with a filter to obtain a poly(styrenesulfonate-perfluorooctene) copolymer {P(SSNa-co-PFO)).
後処理
- temperaturewith heating
- customThe monomers are polymerized for 24 hours or more
- customto sit at ambient temperature
- filtrationfiltered with
- filtrationa filter
出典と根拠
- ORDレコード
- ord-0c8c1e0f5bec43adb00d0ea8fe72e99f
- 出典データセット
- uspto-grants-2011_01
- 特許番号
- US07875208B2
反応ノート
読み込み中…