ホームMCPSkillsワークベンチOpenChem
ホームワークベンチ通知マイページ
llms.txt · skill.md · MCPガイドプライバシーポリシー · 利用規約 · サポートv1.8.5
  1. ホーム
  2. /反応

Isopropanol → Urea

HRID 366285
印刷

反応式

[C:1](=[O:22])(OCCCCCCCCCCCCCCCCCC)[NH2:2].CC(O)C.[NH2:27][CH2:28][CH2:29][CH:30]([NH2:33])[CH2:31][CH3:32].O=C=[N:36]C1CC(C)(C)CC(C)(CN=C=O)C1>CCCCCCC.C1(C)C(C)=CC=CC=1>[NH2:27][CH2:28][CH2:29][CH:30]([NH2:33])[CH2:31][CH3:32].[NH2:36][C:1]([NH2:2])=[O:22]
参加物実験手順後処理出典と根拠反応ノート

参加物

8

反応物 4

HCID 3776IsopropanolHCID 1024441,3-DiaminopentaneHCID 169132Isophorone diisocyanateHCID 233052Octadecyl carbamate

生成物 2

HCID 1176UreaHCID 1024441,3-Diaminopentane

試薬・触媒・溶媒 2

HCID 7237
O-Xylene
溶媒
HCID 8900Heptane溶媒

実験手順

To a solution of 4.4 grams of polyoctadecyl carbamate-co-vinyl acetate having 50 mole % octadecyl carbamate (prepared in xylene at 40 percent solids as described above) and 1.58 grams of polyvinyl butyral (available under the trade designation "BUTVAR" B72 from Monsanto Company, St. Louis, Mo.) in a solvent mixture of 178.6 grams of 2-propanol, 20.6 grams of xylene and 59.9 grams of heptane was added 0.40 grams of 5,000 Mn polydimethylsiloxane diamine (PDMS, prepared following U.S. Pat. No. 5,512,650) and 0.50 grams of 1,3-diaminopentane (available under the trade designation "DYTEK" EP from DuPont) with stirring at 25° C. Next, 1.10 grams of isophorone diisocyanate (IPDI available from Huls or Bayer) was added at 25° C. with stirring and a slow nitrogen purge. The mixture was stirred for 30 minutes, and, in the presence of the polyoctadecyl carbamate-co-vinyl acetate and the polyvinyl butyral, the IPDI reacted with the PDMS diamine and the 1,3-diaminopentane to form a polydiorganosiloxane urea-containing component with 20 weight % PDMS and 80 weight % 1,3-diaminopentane/IPDI. The final product mixture was a homogeneous, hazy, approximately 3% solids solution of a polymer component (polyoctadecyl carbamate-co-vinyl acetate), a polydiorganosiloxane urea-containing component and polyvinyl butyral in a 55:25:20 solids weight ratio.

後処理

  1. customprepared
  2. customa slow nitrogen purge
  3. stirringThe mixture was stirred for 30 minutes
  4. customin the presence of the polyoctadecyl carbamate-co-vinyl acetate and the polyvinyl butyral, the IPDI reacted with the PDMS diamine

出典と根拠

ORDレコード
ord-3839d4b0eebe46a18f1eca0149aec15d
出典データセット
uspto-grants-2000_10
DOI
10.6084/m9.figshare.5104873.v1
特許番号
US06129971

反応ノート

このページの内容参加物実験手順後処理出典と根拠反応ノート