反応式
[P:1]([O-:5])([O-:4])([O-:3])=[O:2].[P:6](=[O:10])([OH:9])([OH:8])[OH:7].[Zr:11]>>[P:1]([O-:5])([O-:4])([O-:3])=[O:2].[Zr+4:11].[P:6]([O-:10])([O-:9])([O-:8])=[O:7].[P:1]([O-:5])([O-:4])([O-:3])=[O:2].[P:1]([O-:5])([O-:4])([O-:3])=[O:2].[Zr+4:11].[Zr+4:11]参加物
4
反応条件
- 温度
- 350 °C
実験手順
A zirconium phosphate film was prepared by adding a stoichometric amount of phosphate in the form of phosphoric acid to a solution of zirconium bound to PEI. The solution was then spin coated onto a glass slide and thermally treated at 1° C. to 120° C. with a dwell time of 30 minutes followed by heating to 350° C. at 1° C./minute with a dwell time of 30 minutes followed by heating to 450° C. at 1° C./minute with a dwell time of 1 hour and then cooling to 25° C.
後処理
- additionthermally treated at 1° C. to 120° C. with a dwell time of 30 minutes
- temperatureby heating to 450° C. at 1° C./minute with a dwell time of 1 hour
- temperaturecooling to 25° C.
出典と根拠
- ORDレコード
- ord-cf4b6531eeb34d11a932e26327e1f566
- 出典データセット
- uspto-grants-2013_09
- 特許番号
- US08530554B1
関連ノート