반응식
CO.[C:3]([O:6][CH:7]=[CH2:8])(=[O:5])[CH3:4].[CH2:9]=[CH:10][S:11]([O-:14])(=[O:13])=[O:12].[Na+:15].CC(N=NC(C#N)(C)C)(C#N)C>O>[C:3]([O:6][CH:7]=[CH2:8])(=[O:5])[CH3:4].[CH2:9]=[CH:10][S:11]([O-:14])(=[O:13])=[O:12].[Na+:15]참가 물질
6
실험 절차
The same vessel as in Example 1 was charged with 130 g. of methanol, 25 g. of water, 320 g. of vinyl acetate, 15 g. of 30% aqueous solution of sodium ethylenesulfonate and 2.8 g. of azobisisobutylonitrile, and polymerization was carried out at a temperature of 70°C. for 3 hours. After adding 2.8 g. of 30% aqueous solution of sodiem ethylenesulfonate to the vessel, the polymerization was further continued for 5 hours to give vinyl acetate-sodium ethylenesulfonate copolymer containing 2.3% by mole of sodium ethylenesulfonate unit. Then the copolymer was hydrolyzed by a conventional method to give a modified PVA of which degree of hydrolysis was 92% by mole.
후처리
- additionThe same vessel as in Example 1 was charged with 130 g
- additionAfter adding 2.8 g
출처 및 근거
- ORD 기록
- ord-f9187d3515574dbcb67370c707e80486
- 출처 데이터셋
- uspto-grants-1976_05
- 특허 번호
- US03959205
연결된 노트
불러오는 중…