Acrylamide → Acrylamide

HRID 1105495

반응식

HRID 1105495 반응식
[C:1]([OH:5])(=[O:4])[CH:2]=[CH2:3].[C:6]([NH2:10])(=[O:9])[CH:7]=[CH2:8].[C:11]([O:15][CH2:16][CH:17]([OH:19])[CH3:18])(=[O:14])[CH:12]=[CH2:13].S(OOS([O-])(=O)=O)([O-])(=O)=O.[NH4+].[NH4+].S([O-])(OCCCCCCCCCCCC)(=O)=O.[Na+:49].[OH-].[Na+]>CO.CC(C)=O>[C:1]([O-:5])(=[O:4])[CH:2]=[CH2:3].[Na+:49].[C:11]([O:15][CH2:16][CH:17]([OH:19])[CH3:18])(=[O:14])[CH:12]=[CH2:13].[C:6]([NH2:10])(=[O:9])[CH:7]=[CH2:8]

참가 물질

10

실험 절차

A terpolymer of sodium acrylate-2-hydroxypropyl acrylate and acrylamide was prepared utilizing an emulsion polymerization process. The mole ratios of acrylic acid to acrylamide, mole percent of 2-hydroxypropyl acrylate and molecular size were varied by controlling the reaction parameters. Six representative samples of the terpolymer were prepared with the compositions of the various terpolymers being estimated based upon their total nitrogen content. In the reaction, ammonium persulfate was utilized as the polymerization initiator or catalyst. Reagent grade acetone and reagent grade anhydrous methanol were utilized to form the solvent. The emulsifier was sodium lauryl sulfate, and 2 N aqueous sodium hydroxide was utilized to neutralize the reactants. The dried products were thereafter milled and passed through a number 30 mesh screen. The reaction was conducted over a period of three hours at a reaction temperature of about 60° C.

후처리

  1. customan emulsion polymerization process
  2. customthe reaction parameters
  3. customSix representative samples of the terpolymer were prepared with the compositions of the various terpolymers
  4. customto form the solvent
  5. customThe dried products were thereafter milled

출처 및 근거

ORD 기록
ord-bba8ba5f4c674effba9024936ea21e88
출처 데이터셋
uspto-grants-1982_01
특허 번호
US04309329

연결된 노트