Nickel → Cobalt dinitrate

HRID 1199629
인쇄

반응식

HRID 1199629 반응식
[Co:1].[Ni:2].[N+:3]([O-:6])([O-:5])=[O:4].[Co+2].[N+:8]([O-:11])([O-:10])=[O:9]>>[N+:3]([O-:6])([O-:5])=[O:4].[Co+2:1].[N+:8]([O-:11])([O-:10])=[O:9].[Co:1].[Ni:2]
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

5

반응물 3

HCID 935NickelHCID 25000Cobalt dinitrateHCID 104730Cobalt

생성물 2

HCID 25000Cobalt dinitrateHCID 10261079Cobalt, compd. with nickel (1:1)

실험 절차

62.5 g of carboxymethyl cellulose was added to 2.5 liters of distilled water and the mixture was kneaded and deaerated to obtain a binder solution. To this binder solution was added 2.5 kg of nickel powder of about 3 μm in average particle size and the mixture was further kneaded and deaerated to obtain a slurry. A wire gauze of 40 meshes was passed through this slurry solution to deposit the slurry thereon and then this wire gauze was passed through a slit to adjust thickness and dried. Thereafter, the wire gauze was sintered at 850° C. in a hydrogen atmosphere to obtain a nickel porous sintered body. Then, an aqueous cobalt nitrate solution was prepared so that addition amount of cobalt based on nickel was 5 atom %. The above nickel porous sintered body was dipped in this aqueous cobalt nitrate solution for 15 minutes and then, was taken out, followed by removing an excess solution and drying. This was sintered at 700° C. in a hydrogen atmosphere to obtain a nickel-cobalt porous sintered body. Another aqueous chromium nitrate solution was prepared so that addition amount of chromium based on nickel was 7 atom %. The above nickel-cobalt porous sintered body was dipped in this aqueous chromium nitrate solution for 15 minutes. Then, this was taken out, followed by removing an excess solution and drying. Thereafter, this was heated at 470° C. in an air atmosphere to oxidize chromium and then was further heated to 700° C. in a hydrogen atmosphere to obtain a nickel-cobalt-chromium oxide ternary anode. Performance of a cell which had the anode obtained in this Example is shown by curve E in FIG. 2. The results were similar to those for the cell where the anode obtained in Example 1 was used.

후처리

  1. customby removing an excess solution
  2. customdrying
  3. customThis was sintered at 700° C. in a hydrogen atmosphere

출처 및 근거

ORD 기록
ord-471807d079c246f382c1e78b566903ec
출처 데이터셋
uspto-grants-1990_02
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US04902587

반응 노트